Huntsman Araldite® PZ 3901 Water-Based Adhesive/Coating
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Base Resin is GT 7071 (Type 1). Typical Solids Content 55%. Mean Particle Size <1µm. Weight per Epoxide (EEW, g/eq), solids basis, 505 to 565. Comments/Applications: Coatings; Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment Excellent stability, small particle size, excellent chemical resistance. Data provided by Ciba Specialty Chemicals.
|
|
|