Huntsman Araldite® XU 3917 Water-Based Adhesive/Coating
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Base Resin is GT 7097 (Type 7). Typical Solids Content 55%. Mean Particle Size <2µm. Weight per Epoxide (EEW, g/eq), solids basis, 2100 to 2600. Comments/Applications: Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment; Coatings Excellent stability, small particle size, excellent adhesion and chemical resistance. Data provided by Ciba Specialty Chemicals.
|
|
|