Huntsman Araldite® XU 3909 Water-Based Adhesive/Coating
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Base Resin is GT 6609 (Type 9). Typical Solids Content 55%. Mean Particle Size <2µm. Weight per Epoxide (EEW, g/eq), solids basis, 2300 to 2800. Comments/Applications: Can/Coil coatings; Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment Highly dilutable, excellent adhesion, flexibility and chemical resistance. Conforms to FDA CFR 175-300. Data provided by Ciba Specialty Chemicals.
|
|
|