Huntsman Araldite® HZ 340 Water-Based Hardener
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Base Resin is Polyamide. Typical Solids Content 50%. Approx. equivalent weight 113. Comments/Applications: Adhesives; Fiber-Sizing; Textiles; Abrasives; Paper treatment; Coatings Solvent free, good adhesion polyamide. For use in coatings for plaster, concrete, masonry, asbestos, cement and nuclear facilities. Data provided by Ciba Specialty Chemicals.
|
|
|