Huntsman Araldite® AER 4100 N80 Brominated Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 330 to 370. Max color is 5. Comments/Applications: Brominated epoxy resin solution in MEK, designed for use in high density multilayer circuit boards exhibiting high glass transition temperature. Data provided by Ciba Specialty Chemicals.
|
|
|