Huntsman Araldite® XB 4383-1 Brominated Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 317 to 345. Max color is 6. Comments/Applications: For use in the manufacturing of thin laminates, prepregs and rigid laminates for printed wiring boards requiring flame retardance. 80% solids in MEK. High performance FR-4 epoxy laminating system. Data provided by Ciba Specialty Chemicals.
|
|
|