Huntsman Araldite® ECN 1280 Epoxy Cresol Novolac
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 212 to 233. Max color is <=6. Comments/Applications: Epoxy cresol novolac with a functionality of 5.1. For high temperature adhesives, coatings, electrical and laminating product areas. Data provided by Ciba Specialty Chemicals.
|
|
|
| Property Data |