Huntsman Araldite® EPN 1180 Epoxy Phenol Novolac
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 175 to 182. Max color is 2. Comments/Applications: Epoxy functionality of 3.6. Much higher viscosity than EPN 1139 or EPN 1179. For higher heat and chemical resistance than PY 307-1 and EPN 1179. Used in matrix applications; filament winding, casting and pultrusion. Data provided by Ciba Specialty Chemicals.
|
|
|