Huntsman Tactix® 138 Epoxy
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 178 to 182. Comments/Applications: Low viscosity epoxy resin for applications such as filament winding. Data provided by Ciba Specialty Chemicals.
|
|
|