Huntsman CY 179 MA Multifunctional Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 131 to 143. Max color is 1. Comments/Applications: Alicyclic diepoxy carboxylate, low viscosity liquid epoxy. High temperature outdoor electrical and casting applications. Long working file, high Tg, brittle. Data provided by Ciba Specialty Chemicals.
|
|
|