Huntsman XB 4122 Multifunctional Resin
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Weight per Epoxide (EEW, g/eq) 330 to 365. Max color is 5. Comments/Applications: Low viscosity, unmodified tough flexible epoxy with excellent workability. For use as a modifier in high solids coatings requiring toughness, adhesion, corrosion and abrasion resistance. Used in matrix applications; filament winding, casting and pultrusion. Data provided by Ciba Specialty Chemicals.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|