Huntsman HY 956 Aliphatic Amine
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Approx. H+ equivalent weight 47. Mix Ratio with GY 6010 is 25. Comments/Applications: Low viscosity liquid amine with low shrinkage, excellent dimensional stability, good electricals. Adhesives, casting, potting, tooling, laminating, coatings. Data provided by Ciba Specialty Chemicals.
|
|
|