Huntsman Euredur® 46 Cycloaliphatic Amine
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Approx. H+ equivalent weight 95. Mix Ratio with GY 6010 is 50. Comments/Applications: Modified polyamine adduct for solvent free coatings, epoxy mortars, lower viscosity and higher chemical resistance. Data provided by Ciba Specialty Chemicals.
|
|
|