Huntsman HY 360 Polyamide
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Approx. H+ equivalent weight 134. Mix Ratio with GY 6010 is 60. Comments/Applications: Very low viscosity, modified polyamidoamine; compatible with bis F resins. Superior chemical resistance. Ultra high solids/solventless coatings. Maintenance and marine primers. Data provided by Ciba Specialty Chemicals.
|
|
|