Huntsman HY 815 US Polyamide
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Approx. H+ equivalent weight 150. Mix Ratio with GY 6010 is 81. Comments/Applications: Solvent free, high molecular weight, low amine content. Superior adhesion, easily pigmented. Trade sale paint enamels. Industrial maintenance, FDA. Flexible mix ratio. Usually used with "Type 1" epoxy resins. Data provided by Ciba Specialty Chemicals.
|
|
|