Huntsman HY 840 US Polyamide
Subcategory: Epoxy; Adhesive; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Approx. H+ equivalent weight 130. Mix Ratio with GY 6010 is 81. Comments/Applications: Solvent free, low viscosity, high amine content with higher flexibility and toughness. Flexible mix ratio 33 - 100 PHR, with GY 6010. High solids or solvent free industrial coatings, adhesives, general purpose industrial. Data provided by Ciba Specialty Chemicals.
|
|
|