Huntsman HZ 340 Polyamide
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Approx. H+ equivalent weight 113. Mix Ratio with GY 6010 is 120. Comments/Applications: Solvent free, water-based polyamide with good adhesion. For use in coatings for plaster, concrete, masonry, asbestos, cement and nuclear facilities. Data provided by Ciba Specialty Chemicals.
|
|
|