Huntsman HT 9506 Special Hardner
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Mix Ratio with GY 6010 is 35. Comments/Applications: Finely ground HT 939. Adhesives, tooling, vinyl plastisols, dipping compounds. Data provided by Ciba Specialty Chemicals.
| Available Properties |
- Maximum Service Temperature, Air
- Processing Temperature
|
|
|
|