Huntsman DT 3126-2 Epoxy Accelerator
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Comments/Applications: Granular solid. Powder coating accelerator for epoxy/COOH functional polyesters, used at 2-3% levels. Data provided by Ciba Specialty Chemicals.
|
|
|