Huntsman DY 062 Epoxy Accelerator
Subcategory: Epoxy; Thermoset
Close Analogs: Ciba Specialty Chemicals has been acquired by Huntsman.
Material Notes: Mix Ratio with GY 6010 is 5. Comments/Applications: Reduces gel time and cure schedule for adhesives and other fast cure epoxy systems. Benzyl dimethyl amine (BDMA)-tertiary amine accelerator. Compatible with anhydride and polyamide hardeners. Flexible mix ratio = 0.5 - 10.0 PHR, with GY 6010. Data provided by Ciba Specialty Chemicals.
|
|
|