GY-70 (Celanese) Carbon Fibers
Subcategory: Carbon Fiber/Thermoset Composite
Key Words: composites, fibers
Material Notes: Polyacrylonitrile fibers are converted into carbon fibers through oxidation in air between 200 - 300°C, followed by carbonization and then graphitization in inert atmospheres at temperatures up to 3000°C.