Phenolic 40%, Carbon fabric 60%
Subcategory: Phenolic; Thermoset; Carbon Fiber/Thermoset Composite
Key Words: composites, fibers
Material Notes: Phenolic - Monsanto "SC 1008". Carbon fabric - "CCA-1"
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Compressive Modulus
|
|
|
|