COIM LARIPUR® LPR5520 Standard Adipate Ester Polyurethane
Subcategory: Polyester, TP; Polyurethane, TP; Thermoplastic
Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:- Excellent abrasion resistance
- Great flexibility with constancy at temperature variations
- Good compression resistance
- Good water and light resistance
- Good resistance to oils, fats and to many types of solvents
Series 20 Standard Adipate Ester: These products are based on saturated polyesters. They exhibit strength and durability with excellent tear and abrasion resistance; good hydrolytic stability resistance to solvents, oxidation and UV light degradation. Information provided by P.A.T. Products, Inc.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Flexural Modulus
- Tear Strength
- Abrasion
- Torsional Stiffness
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|