COIM LARIPUR® LPR2203-93A Seal Grade TPU
Subcategory: Polyether; Polyurethane, TP; Thermoplastic
Material Notes: Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:- Excellent abrasion resistance
- Great flexibility with constancy at temperature variations
- Good compression resistance
- Good water and light resistance
- Good resistance to oils, fats and to many types of solvents
Seal Grade TPU Products: These products were specially developed for manufacturing hydraulic gaskets or any other heavy-duty application requiring high compression resistance even at high temperature and/or in contact with oils and fats. Two products based on polycaprolactone polyester, E 2202-95A and E 107-93A, and one based on PTMG polyether, E 2203-93A. Information provided by P.A.T. Products, Inc.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- 50% Modulus
- 100% Modulus
- 300% Modulus
- Flexural Modulus
- Tear Strength
- Abrasion
- Compression Set
- Compression Set, Elevated Temperature
- Vicat Softening Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|