COIM FILCO® 306 Film Former for Glass Fiber Sizes

 

Subcategory: Additive/Filler for Polymer; Thermoplastic

Material Notes:
Description: Film Former for Glass Fiber Sizes
General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat.
Typical Physical and Chemical Characteristics:

  • Filco 306 is an epoxy resin in non-ionic water emulsion
  • pure epoxy resin
  • epoxy equivalent ~ 330
  • narrow particle size distribution
  • hydrolysis and sedimentation stability from pH 2 to 12 min. 48 h
  • good shelf life
  • high mechanical shear stability of the diluted emulsion

Characteristics of the dried film:
  • clear
  • tacky film
  • film less soft then the film for Filco 309
  • compatible with unsaturated polyester, epoxy, phenolic matrices
  • quickly soluble in styrene

Applications: Filco 306 is suggested as a film former for glass fiber sizes for:
  • filament winding roving
  • pultrusion roving
  • woven roving

Information provided by P.A.T. Products, Inc.

Available Properties
  • Solids Content
  • Particle Size
  • pH
  • Viscosity
  • Appearance
  • Epoxy Equivalent on Dry Resin
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。