COIM FILCO® 339 Film Former for Glass Fiber Sizes
Subcategory: Additive/Filler for Polymer; Thermoplastic
Material Notes: Description: Film Former for Glass Fiber Sizes General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat. Typical Physical and Chemical Characteristics: Filco 339 is an unsaturated polyester-epoxy polymer in non-ionic water emulsion Characteristics of the dried film: - clear
- not tacky
- compatible with unsaturated polyester and epoxy resins
- very quickly soluble in styrene
Applications: Filco 339 is suggested as a film former for glass fiber sizes for:- roving for translucent sheet
- spray roving
- mat roving
Fiber glass sized with Filco 339 present high impregnation speed during glass resin composite high transparency. Information provided by P.A.T. Products, Inc.
| Available Properties |
- Solids Content
- Particle Size
- pH
- Appearance
- Epoxy Equivalent on Dry Resin
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|