COIM FILCO® 350 Non Ionic Unsaturated Polyester Polymer Aqueous Emulsion for Glass Fiber Sizing
Subcategory: Additive/Filler for Polymer; Thermoplastic
Material Notes: Description: Non Ionic Unsaturated Polyester Polymer Aqueous Emulsion for Glass Fiber Sizing General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat. Applications: Filco 350 has been studied as a primary film forming component of glass fiber sizing for unsaturated polyester matrix strengthening. Consider the following special properties:- pseudo-glass consistency of film
- good solubility in vinylic solvents
- good compatibility with other typical sizing component formulations
- good compatibility with various unsaturated polyester matrixes
- good transparency of reinforced compounds
- high impregnation speed of sized fibers during glass/resin compound preparation
It is recommendable to use Filco 350 in combination with metacrylic radical organosilanes for glass fiber sizing formulation for:- roving for translucent sheets
- roving for chip/spray
- chopped strand mat with powder and liquid binder highly soluble in styrene
Information provided by P.A.T. Products, Inc.
| Available Properties |
- Solids Content
- pH
- Brookfield Viscosity
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|