COIM FILCO® 362 Film Former for Glass Fiber Sizes
Subcategory: Additive/Filler for Polymer; Thermoplastic
Material Notes: Description: Film Former for Glass Fiber Sizes General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat. Typical Physical and Chemical Characteristics: - Filco 362 is an epoxy-resin in non ionic water emulsion
- non ionic emulsifier built in the polymer
- narrow particle size distribution
- good shelf life owing to hydrolytic resistance and fine particle size
- high mechanical shear stability to the diluted emulsion
- hydrolysis and sedimentation stability in a wide pH range
Characteristics of the dried film: - clear
- non tacky
- glass transition temperature TG " 10°C
- high thermal stability
- does not yellow at high temperature
- compatible with epoxy and all types of unsaturated polyesters
- quickly soluble in styrene
Applications: Filco 362 is suggested as a film former for glass fiber sizes for:- chopped strand for thermoplastic matrices (PBT-PC-ABS, etc.)
- filament winding roving
- pultrusion roving
- roving for translucent sheet
Information provided by P.A.T. Products, Inc.
| Available Properties |
- Solids Content
- Particle Size
- pH
- Viscosity
- Acid Value
- Appearance
- Epoxy Equivalent on Dry Resin
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|