COIM FILCO® 650 Film Former for Glass Fiber Sizes
Subcategory: Additive/Filler for Polymer; Thermoplastic
Material Notes: Description: Film Former for Glass Fiber Sizes General Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in powder and emulsion form and are collectively known as FILCO®. The products in the FILCO® line serve to size glass fiber, to optimize the mechanical characteristics of the fiber, or to bind the fibers for the production of mat. Typical Physical and Chemical Characteristics: Filco 650 is an unsaturated modified polyester polymer in a non ionic water emulsion. Characteristics of the dried film: - clear
- non tacky
- compatible with unsaturated polyester and other thermosets
- low soluble in styrene
Applications: Filco 650 is suggested as a binder for performs and c.s. mat with low solubility in styrene. The use of organic peroxide as a source of free radicals is suggested. Benzoyl peroxide in water dispersion can for example be used at a level of 0.5 - 1.0% on Filco 650. Filco 650 is also suggested as a film former for glass fiber sizes for: Information provided by P.A.T. Products, Inc.
| Available Properties |
- Solids Content
- Particle Size
- pH
- Viscosity
- Appearance
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|