Colorite Polymers Flexchem 5551-02 Vinyl Compound

 

Subcategory: Vinyl; Thermoplastic

Material Notes:
Description: The Flexchem "51" series is a group of translucent, flexible, non-toxic vinyl compounds which were specifically developed to replace silicone in various applications. These compounds utilize a non-phthalate plasticizer system for use in medical device applications. This unique product line offers excellent release characteristics, rubber-like compression properties, good burst strength and durability. These compounds can even be solvent bonded for ease of assembly. Flexchem compounds can be extruded or injection molded; they do not require any special equipment for processing. A replacement for silicone in a nearly endless list of uses, including tubing for pumping applications, urinary drain sets, beverage spouts, gaskets, etc., Flexchem is available in durometers ranging from 35 to 65 shore A hardness. It is formulated utilizing only FDA sanctioned raw materials and has been designed for use in USP Class VI applications. For medical use, complete traceability and lot identification of all components in the Flexchem products are maintained at Colorite.

Information provided by Colorite Polymers.

Available Properties
  • Specific Gravity
  • Hardness, Shore A
  • Tensile Strength, Ultimate
  • Elongation at Break
  • 100% Modulus
  • Compression Set
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。