Colorite Polymers 8033SF General Purpose Vinyl Compound
Subcategory: Vinyl; Thermoplastic
Material Notes: Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame retardance, low temperature, or chemical resistance, are all available. Formulations for exterior or interior use. Typical Applications: General Purpose Low Gloss Extrusion Information provided by Colorite Polymers.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- 100% Modulus
|
|
|
|