CoolPoly® D5108 Thermally Conductive Polyphenylene Sulfide
Subcategory: Polyphenylene Sulfide; Thermoplastic; Polymer
Material Notes: CoolPoly D series of thermally conductive plastics transfers heat, a characteristic previously unavailable in injection molding grade polymers. CoolPoly is lightweight, netshape moldable and allows design freedom in applications previously restricted to metals. The D series is electrically non-conductive and can be used for its dielectric properties.CoolPoly D5108 is a thermally conductive injection molding resin based on a polyphenylene sulfide (PPS) matrix. CoolPoly D5108 is electrically insulative. Thermally conductive polymers like CoolPoly D5108 cool faster than standard injection molding grade resins. Information provided by Cool Polymers, Inc.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Arc Resistance
- High Voltage Arc Resistance to Ignition (HVAR)
- Comparative Tracking Index
- Hot Wire Ignition, HWI
- High Voltage Arc-Tracking Rate, HVTR
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Specific Heat Capacity
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Moisture Content
- Dew Point
- Injection Pressure
- Hold Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|