Quantum Composites Lytex® 9063 63% Glass Fiber Epoxy SMC
Subcategory: Epoxy; Composite SMC; Thermoset; Polymer
Close Analogs: 14 Composite SMCs from Quantum Composites are listed in MatWeb. Data provided by the manufacturer.
Key Words: Sheet Molding Compound
Material Notes: Lytex 9063 is a high performance, glass fiber reinforced epoxy sheet molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and excellent electrical properties. It meets the requirements of MIL-M-46069 and MIL-M-46892. Form and Color = Sheet, Black. Glass Length (Std.) = 0.5"
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Izod Impact, Notched
- Electrical Resistivity
- Dielectric Constant
- Dielectric Strength
- Dissipation Factor
- Maximum Service Temperature, Air
- Shrinkage
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|