Quantum Composites QC-3450 48% Glass Fiber High Temperature Use SMC
Subcategory: Composite SMC; Thermoset; Polymer
Close Analogs: 14 Composite SMCs from Quantum Composites are listed in MatWeb. Data provided by the manufacturer.
Key Words: Sheet Molding Compound
Material Notes: QC-3450 is highly reinforced with glass fibers. It is designed for compression molding of components requiring high structural strength and good resistance to elevated temperatures. Long-term use temperature is around 375°F. Form and Colors = Rolled Sheet, Black/Natural. Glass Fiber Length = .5 inch.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Shrinkage
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|