Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC
Subcategory: Vinyl Ester; Composite SMC; Thermoset; Polymer
Close Analogs: 14 Composite SMCs from Quantum Composites are listed in MatWeb. Data provided by the manufacturer.
Key Words: Sheet Molding Compound
Material Notes: QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temperatures above 125°C, and will withstand short term exposures at over 300°C. Form and Color = Rolled Sheet, Green/Gray/Black. Glass Fiber Length = 1 inch.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Maximum Service Temperature, Air
- Glass Temperature
- Shrinkage
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|