Cotronics Duralco™ 127 400°F (200°C) Graphite Filled Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: One component, graphite filled epoxy for low cost production applications. Can be used with automatic dispensing equipment.
| Available Properties |
- Viscosity
- Volume Resistivity
- Thermal Conductivity
- Maximum Service Temperature, Air
- Cure Time
|
|
|
|