Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy
Subcategory: Epoxy; Thermoset
Material Notes: Two component, heat curing, aluminum filled epoxy suitable for high temperature tooling and a readily machinable repair or construction material. Similar to Duralco™ 132, but with a maximum service temperature of 600°F (315°C). Cures with mild heat.