Cotronics Duralco™ 4538N Super Flexible Epoxy, Room Temperature Cure
Subcategory: Epoxy; Thermoset
Material Notes: Rubber-like epoxy that has the flexible of a silicone and the chemical stability of an epoxy. It adheres to most plastics, metals, ceramics, glass, rubber and even treated Teflon™. Cures at room temperature. Will not soften or gum up in use. 4528N is resistant to thermal shock and vibration, chemicals, solvents and electricity. Provides class “H” service. Applications: stress free bonding and flexible encapsulations.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Cure Time
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|