Cotronics Duralco™ 4703 Adhesive and Tooling Compound
Subcategory: Epoxy; Thermoset
Material Notes: High temperature resin reinforced with ceramic and metallic fibers and particles, resulting in high thermal stability. Easily machined to close tolerances and will repair and rebuild worn or cracked composites, dies, fixtures, jigs, etc. Electrically non-conductive. Corrosion Resistance: resistant to most chemicals, solvents, acids and bases.
| Available Properties |
- Density
- Moisture Absorption at Equilibrium
- Viscosity
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Volume Resistivity
- Dielectric Strength
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
- Shrinkage
- Cure Time
|
|
|
|