CPC - Vycom CELTEC® Expanded Rigid foam PVC board
Subcategory: Vinyl; Thermoplastic
Material Notes: Celtec Displayboard is a foamed polyvinyl chloride (PVC) sheet whose extraordinary combination of features makes it ideal for signage, exhibits, store displays, POP, Kiosks, screen printing and more. The surface is a smooth matte finish that makes it ideal to paint or laminate to secondary substrates. Celtec also has good screw and staple retention which makes it ideal for stage prop design, cabinetry and other wood replacement projects. Sheets are tough, high-strength and lightweight, and can be ordered in a wide range of sizes, thicknesses and colors. Celtec sheets are free of lead, cadmium, barium and zinc. Celtec is recommended for industrial and commercial signage. It readily accepts virtually any form of graphic overlay (print, paint and photo mounting). Celtec is also easy to cut and shape, making it a strong choice for three-dimensional exhibits, displays and stage sets.FEATURES AND BENEFITS - Lightweight- Celtec is easy to handle, easy to work with.
- Low Flammability- Celtec meets UL94 5V, UL 1975 and has a flame spread of 20 according to ASTM E84.
- Water resistant- Celtec has a closed cell structure and has extremely low water absorption values.
- Surface- Celtecs smooth matte surface is ideal for graphics, printing and laminating.
- Weatherability- Celtec is more color-fast than other foam PVC products.
- Strength- Celtec has an excellent strength to weight ratio as shown in the screw and staple pull test data.
- Thermal Conductivity- Celtec has excellent insulating characteristics.
- Safety- Celtec contains no lead, cadmium or zinc.
Information provided by Compression Polymers Corp - Vycom
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Unnotched
- Gardner Impact
- Izod Impact, Notched
- Dielectric Strength
- CTE, linear 68°F
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Flame Spread Index
- Burning Rate
- Foam Fire
- Nail Hold, Lbf/in penetration
- Oil Canning; (at 140°F) 10mm - 25mm
- Screw Hold, Lbf/in penetration
- Staple Hold, Lbf/in penetration
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|