CPC - Vycom FLAMETEC™ CP7-D Flame Retardant Polypropylene
Subcategory: Polypropylene; Thermoplastic
Material Notes: Flametec™ CP7-D is a proprietary designation for a flame retardant polypropylene formulation. CP7-D represent our version of polypropylene sheet whose flame retardant characteristics meet or exceed the most rigorous FMRC 4910 testing standards for most aspects of flame retardation, self-extinguishing characteristics and burnthrough. In addition, CP7-D also meets or exceeds test standards for low smoke generation and minimal toxic by-products. CP7-D is a filled PP sheet material, therefore, chemical compatibility should be verified for each application.FEATURES AND BENEFITS - Impact Strength- Flexibility and strength of designs vs. other FRPP products.
- Weldability- Easy to fabricate with conventional welding equipment.
- Economics- An economical alternative for fire safe construction.
- Fire Safe- Listed in accordance to FMRC 4910, fire safe materials for clean room construction.
- Extruded Sheet- Offers the best gauge consistency, surface and tolerances.
Information provided by Compression Polymers Corp - Vycom
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Yield
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Vicat Softening Point
- Flammability, UL94
- Flammability Test
- Corner Weld Strength, lb/in
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|