CPC - Vycom HITEC® Pipe Grade HDPE High Density Polyethylene
Subcategory: Polyethylene; Thermoplastic; HDPE
Material Notes: Hitec pipe grade HDPE is a special formulation that has high impact strength, and environmental stress crack resistance. Hitec Pipe grade meets Federal specification L-P 390C, ASTM D1248 Type III weather resistant black and ASTM 3350 cell class 345464C.FEATURES AND BENEFITS - Hardness- Hitec Pipe Grade is abrasion resistant and will resist scratching.
- Strength- Hitec Pipe Grade has high tensile and stiffness for machine parts and tank applications.
- Ductility- Hitec Pipe Grade is stress crack resistant.
- Machinable- Hitec Pipe Grade is easy to machine with conventional tools.
Information provided by Compression Polymers Corp - Vycom
| Available Properties |
- Density
- Environmental Stress Crack Resistance
- ESCR 100% Igepal®
- Hardness, Rockwell L
- Hardness, Shore D
- Tensile Strength, Ultimate
- Elongation at Break
- Flexural Modulus
- 2% Secant Modulus
- Izod Impact, Notched
- Hydrostatic Design Basis @ 73°F
- CTE, linear 68°F
- Melting Point
- Vicat Softening Point
- Brittleness Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|