CPC - Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride

 

Subcategory: Vinyl; Thermoplastic

Material Notes:
Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose extraordinary combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed cell structure does not absorb water and acts as a water barrier. Because of its staple pull and screw pull strength, Celtec Marine is ideal for applications in marine upholstery, seat backs, seat bottoms, trim for rough fiberglass openings, brackets, cabinets, draws etc.

FEATURES AND BENEFITS

  • Light weight- Celtec marine combines lightweight with strength to reduce weight in boat construction.
  • Strength- Celtec Marine has a high strength to weight ratio that makes it ideal for many boat building applications.
  • Superior workability- Celtec marine is easy to form, cut, glue, screw, nail, and staple.
  • Flammability- Celtec Marine meets UL guidelines, is self extinguishing and has a flame spread of 20.
  • Thermal conductivity- Celtec Marine is an excellent insulator.
  • Weatherability and water resistance- Celtec Marine is durable and will not absorb water.
  • Density- Celtec Marine is lighter than water and it floats.
  • Safety- Celtec Marine is Lead, cadmium, barium and zinc free.
  • Stability- Celtec Marine will not rot and it is cleanable and retains its color.
  • Economical- Celtec Marine is designed to last and it is economical to use.

Information provided by Compression Polymers Corp - Vycom

Available Properties
  • Density
  • Water Absorption
  • Tensile Strength, Ultimate
  • Tensile Modulus
  • Flexural Modulus
  • Flexural Strength
  • Charpy Impact, Unnotched
  • Gardner Impact
  • CTE, linear 68°F
  • Deflection Temperature at 1.8 MPa (264 psi)
  • Flame Spread Index
  • Burning Rate
  • Nail Hold, Lbf/in penetration
  • Screw Hold, Lbf/in penetration
  • Staple Hold, Lbf/in penetration
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。