CPT C-Flex® R70-072 Opaque Biocompatible TPE
Subcategory: Elastomer, TPE; Thermoplastic
Key Words: SEBS
Material Notes: C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current United States Pharmacopoeia Class VI test requirements. C-Flex® does not contain latex rubber, polyvinyl chloride, silicone rubber, or polyurethane.Information provided by Consolidated Polymer Technologies.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Melt Flow
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Tear Strength
- Taber Abrasion, mg/1000 Cycles
- Compression Set
- Compression Set, Elevated Temperature
- Tensile Set
- Brittleness Temperature
- Processing Temperature
- Middle Barrel Temperature
- Drying Temperature
- Injection Pressure
- Sterilization methods:
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|