Cresset Powers Cress-Alon™ A3000 3.0 r.v. Film or Extrusion Grade Nylon 6, 50% RH
Subcategory: Nylon; Thermoplastic; Nylon 6
Material Notes: Neat resin, for film or extrusion.Information provided by Cresset Powers Ltd.
| Available Properties |
- Density
- Apparent Bulk Density
- Viscosity Measurement
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Flexural Modulus
- Flexural Yield Strength
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Moisture Content
- Extractables, wt%
|
|
|
|