CRP Technology WindForm GF Polyamide-Aluminum-Glass Composite
Subcategory: Nylon; Thermoplastic; Nylon 12; Polymer
Material Notes: Rapid Prototyping (Layer Manufacturing Technique) represents the most advanced technique in obtaining, in rapid timing, the finished testing model. Windform™ is a unique product within the prototyping sector. There is not any one product on the market which has any of Windform's characteristics or comes close to its performance. Class of material: Composite polyamide based powder Technology: Selective Laser Sintering WindForm™ GF Light Grey coloured composite polyamide based material, with added aluminium and glass, with improved heat deflection temperature (HDT) and superior stiffness, excellent surface finish, wear resistance and first-rate detail reproduction. WindForm™ GF offers an attractive, gleaming metallic look, valuable in many applications, such as wind tunnel, in design and functional applications. WindForm™ GF absorbs slightly less liquid compared to the other WindForm™ products and is particularly suitable for applications which require a superior surface finish. Applications: Functional objects, Intake manifold (aspiration and cooling ducts, air intake), hydraulic ducts (Fluid/flowing temperature up to 125 centigrade degrees), Fuel Systems, household appliances. These uses are only an examples. The product's versatility together with the technology used allow countless possibilities of utilization in areas such as aerospace, racing, motorsports, automotive, design, packaging, electronics, entertainment, government, consumer products (household appliances), industrial, lighting systems, OEM products, etc. Information provided by CRP Technology.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact Unnotched
- Charpy Impact, Notched, Low Temp
- Charpy Impact, Notched
- Volume Resistivity
- Surface Resistance
- Melting Point
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Color
- Surface Finish
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|