CYRO Cyrolon® AR Polycarbonate Sheet
Subcategory: Polycarbonate; Thermoplastic
Material Notes: Data provided by CYRO Industries Continuously manufactured sheet with better impact and heat resistance than typical acrylic sheet. Offers protection against weathering. Used for windows, skylights, signs, displays, vending machine panels, machine guards, safety glazing, and bus shelters.
| Available Properties |
- Water Absorption
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Impact Test
- Electrical Resistivity
- Dielectric Constant
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor
- Dissipation Factor, Low Frequency
- CTE, linear 20°C
- Thermal Conductivity
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability, UL94
- Oxygen Index
- Refractive Index
- Transmission, Visible
- Processing Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|