Cyro Europlex® Clear HC 99710 Transparent Film
Subcategory: Acrylic; Thermoplastic; Polymer
Material Notes: EUROPLEX® Film HC 99710 is a highly transparent, very efficient weather and UV protection film with excellent surface properties such as chemical resistance, anti-graffiti and dirt-repellent behavior. EUROPLEX® Film HC 99710 is based on a special polymethyl methacrylate (PMMA) formulation with outstanding weather resistance, extremely high UV absorption as well as superior printability and lamination performance. It owes these extraordinary surface properties to the polyvinylidene fluoride (PVDF) layer which is fused to the PMMA substrate.Information provided by Cyro Industries
| Available Properties |
- Density
- Surface Tension
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Haze
- Yellow Index
- Transmission, Visible
- UV Transmittance
- Chemical Resistance to Alcohol
- Chemical Resistance to Benzene
- Chemical Resistance to Ethyl Acetate
- Chemical Resistance to Hexane
- Chemical Resistance to Methyl Ethyl Ketone
- Chemical Resistance to Naphtha
- Chemical Resistance to THF
- Chemical Resistance to Toluene
- Weather Resistance, Xenotest 1200/5000hr
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|