Cyro Rohaglas® Clear 99524 Acrylic Film
Subcategory: Acrylic; Thermoplastic; Polymer
Material Notes: ROHAGLAS® Film 99524 acrylic film, based upon polymethyl methacrylate and acrylic elastomers, offers crystal-clear optical properties with two glossy (Class A) surfaces. Its excellent abrasion resistance, combined with long-term outdoor weatherability offers outstanding performance as a decor carrier and as a substrate surface protector. ROHAGLAS 99524 film has superior processability in die-cutting and all forming processes. In addition, it presents good resistance towards weak acids and alkalis as well as non-polar solvents.Information provided by Cyro Industries
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Volume Resistivity
- Surface Resistance
- Dissipation Factor
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
- Vicat Softening Point
- Refractive Index
- Haze
- Yellow Index
- Transmission, Visible
- UV Transmittance
- Birefringence ASTM D4093
- Pencil Hardness
- Weather Resistance, Xenotest 1200/5000hr
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|