Cyro Paraglas Soundstop® GS CC Transparent Sheet
Subcategory: Acrylic; Thermoplastic
Material Notes: Paraglas Soundstop GS CC sheet incorporates polyamide filaments and is typically used on bridges and overpasses. In the event of impact by a car or truck, the imbedded filaments will hold the broken sheet, preventing pieces from falling below.Information provided by Cyro Industries
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Charpy Impact Unnotched
- CTE, linear 20°C
- Maximum Service Temperature, Air
- Deflection Temperature at 1.8 MPa (264 psi)
- Vicat Softening Point
- Flammability Test
- Refractive Index
- Haze
- Yellow Index
- Transmission, Visible
- Resistance to Brushfire
- Resistance to stone projectiles
- Self Ignition Temperature °F
- Smoke Density, % (15mm thick)
- Sound Transmission Loss, dB (15mm)
- Sound Transmission Loss, dB (20mm)
- Sound Transmission Loss, dB (25mm)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|